Poor photo quality...sorry about that.
Writing samples were done using a "Ta-tung 717" FP, unless stated otherwise.
Writing samples were done with a 0.7mm loose FP nib in a dip pen holder, dipped in the inks. The photo looks pretty accurate on me screen, but ymmv.
Paper used is Rhodia #16 graph.
And here is the water resistance test. I soaked the section on the left in water for 10 minutes, and water droplets were flicked onto the section on the right.